Standard

Unoccupied states evolution with oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(100) surfaces. / Moller, PJ; Komolov, SA; Lazneva, EF; Komolov, AS.

в: Applied Surface Science, Том 175, 15.05.2001, стр. 663-669.

Результаты исследований: Научные публикации в периодических изданияхстатьяРецензирование

Harvard

Moller, PJ, Komolov, SA, Lazneva, EF & Komolov, AS 2001, 'Unoccupied states evolution with oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(100) surfaces', Applied Surface Science, Том. 175, стр. 663-669.

APA

Vancouver

Author

Moller, PJ ; Komolov, SA ; Lazneva, EF ; Komolov, AS. / Unoccupied states evolution with oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(100) surfaces. в: Applied Surface Science. 2001 ; Том 175. стр. 663-669.

BibTeX

@article{3ad490205833415091fe9b12db14842b,
title = "Unoccupied states evolution with oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(100) surfaces",
abstract = "An unoccupied density of states (DOS) evolution under oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(1 0 0)-(2 x 2) substrates are investigated. The metal deposition and subsequent oxidation were studied in situ under UHV conditions by means of LEED, AES, TCS and work function measurements. An appearance of metal- and oxygen-derived bands of the unoccupied DOS was traced in the TC spectra. Metal oxidation was followed by the hybridization of metal and oxygen orbitals and by the appearance of the mainly O 2p oxygen-derived bands, which are characterized by a set of DOS maxima, located at the following energies (above the Fermi level): 8.0, 11.5, 14.3, 15.0 and 19.0 eV for MgO; 6.0, 8.1, 16.8 and 20.5 eV for ZnO and 7.5, 10.0 and 12.7 eV for CdO. The results obtained are discussed in comparison with previously published experimental and theoretical data on unoccupied DOS in metal oxides. (C) 2001 Elsevier Science B.V. All rights reserved.",
keywords = "density of unoccupied states, metal oxide surfaces, total current spectroscopy, TOTAL CURRENT SPECTROSCOPY, X-RAY-ABSORPTION, ELECTRONIC-STRUCTURE, OXIDE, GROWTH",
author = "PJ Moller and SA Komolov and EF Lazneva and AS Komolov",
year = "2001",
month = may,
day = "15",
language = "Английский",
volume = "175",
pages = "663--669",
journal = "Applied Surface Science",
issn = "0169-4332",
publisher = "Elsevier",
note = "null ; Conference date: 09-07-2000 Through 13-07-2000",

}

RIS

TY - JOUR

T1 - Unoccupied states evolution with oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(100) surfaces

AU - Moller, PJ

AU - Komolov, SA

AU - Lazneva, EF

AU - Komolov, AS

PY - 2001/5/15

Y1 - 2001/5/15

N2 - An unoccupied density of states (DOS) evolution under oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(1 0 0)-(2 x 2) substrates are investigated. The metal deposition and subsequent oxidation were studied in situ under UHV conditions by means of LEED, AES, TCS and work function measurements. An appearance of metal- and oxygen-derived bands of the unoccupied DOS was traced in the TC spectra. Metal oxidation was followed by the hybridization of metal and oxygen orbitals and by the appearance of the mainly O 2p oxygen-derived bands, which are characterized by a set of DOS maxima, located at the following energies (above the Fermi level): 8.0, 11.5, 14.3, 15.0 and 19.0 eV for MgO; 6.0, 8.1, 16.8 and 20.5 eV for ZnO and 7.5, 10.0 and 12.7 eV for CdO. The results obtained are discussed in comparison with previously published experimental and theoretical data on unoccupied DOS in metal oxides. (C) 2001 Elsevier Science B.V. All rights reserved.

AB - An unoccupied density of states (DOS) evolution under oxidation of ultrathin Mg, Zn and Cd layers on SrTiO3(1 0 0)-(2 x 2) substrates are investigated. The metal deposition and subsequent oxidation were studied in situ under UHV conditions by means of LEED, AES, TCS and work function measurements. An appearance of metal- and oxygen-derived bands of the unoccupied DOS was traced in the TC spectra. Metal oxidation was followed by the hybridization of metal and oxygen orbitals and by the appearance of the mainly O 2p oxygen-derived bands, which are characterized by a set of DOS maxima, located at the following energies (above the Fermi level): 8.0, 11.5, 14.3, 15.0 and 19.0 eV for MgO; 6.0, 8.1, 16.8 and 20.5 eV for ZnO and 7.5, 10.0 and 12.7 eV for CdO. The results obtained are discussed in comparison with previously published experimental and theoretical data on unoccupied DOS in metal oxides. (C) 2001 Elsevier Science B.V. All rights reserved.

KW - density of unoccupied states

KW - metal oxide surfaces

KW - total current spectroscopy

KW - TOTAL CURRENT SPECTROSCOPY

KW - X-RAY-ABSORPTION

KW - ELECTRONIC-STRUCTURE

KW - OXIDE

KW - GROWTH

M3 - статья

VL - 175

SP - 663

EP - 669

JO - Applied Surface Science

JF - Applied Surface Science

SN - 0169-4332

Y2 - 9 July 2000 through 13 July 2000

ER -