The influence of ultra fine grained (UFG) and coarse grained (CG) microstructure of the titanium alloy Ti-6Al-4V on the strength of a diffusion bonded (DB) joint was studied using a laboratory DB fixture and a new shear test rig. The DB process was carried out at 725 °C and 825 °C during 2 and 4 h in a vacuum furnace. Coarsening of grain structure resulting from different DB cycles was quantified. The chain pores were observed at 725 °C for both microstructure conditions bonded during 2 h. The increase of bonding time up to 4 h leads to subsequent elimination of the pores. The UFG samples bonded at 725 °C showed a higher level of the shear strength than CG samples for both bonding times. The CG material demonstrated the highest shear strength after 4 h of DB bonding at 825 °C. The increase of the creep deformation of UFG samples when compared to the CG condition was observed as a result of DB at of 725 °C during 4 h.
Язык оригинала | английский |
---|---|
Страницы (с-по) | 251-258 |
Число страниц | 8 |
Журнал | Materials Science and Engineering A |
Том | 726 |
DOI | |
Состояние | Опубликовано - 30 мая 2018 |
Опубликовано для внешнего пользования | Да |
ID: 35168457