Strain rate sensitivity studies in an ultrafine-grained Al-30wt.% Zn alloy using micro- and nanoindentation. / Chinh, Nguyen Q.; Csanádi, Tamás; Gyori, Tivadar; Valiev, Ruslan Z.; Straumal, Boris B.; Kawasaki, Megumi; Langdon, Terence G.
In: Materials Science and Engineering A, Vol. 543, 01.05.2012, p. 117-120.Research output: Contribution to journal › Article › peer-review
}
TY - JOUR
T1 - Strain rate sensitivity studies in an ultrafine-grained Al-30wt.% Zn alloy using micro- and nanoindentation
AU - Chinh, Nguyen Q.
AU - Csanádi, Tamás
AU - Gyori, Tivadar
AU - Valiev, Ruslan Z.
AU - Straumal, Boris B.
AU - Kawasaki, Megumi
AU - Langdon, Terence G.
PY - 2012/5/1
Y1 - 2012/5/1
N2 - The characteristics of plastic deformation of an ultrafine-grained (UFG) Al-30. wt.% Zn alloy were investigated using depth-sensing micro- and nanoindentation. Emphasis was placed on the effects of grain boundaries and the unusually high strain rate sensitivity. It is shown that there is a close relationship between enhanced strain rate sensitivity and ductility in this UFG material and this is associated with grain boundary sliding and enhanced diffusion along the Al/Al grain boundaries which appear to be wetted by Zn-rich layers.
AB - The characteristics of plastic deformation of an ultrafine-grained (UFG) Al-30. wt.% Zn alloy were investigated using depth-sensing micro- and nanoindentation. Emphasis was placed on the effects of grain boundaries and the unusually high strain rate sensitivity. It is shown that there is a close relationship between enhanced strain rate sensitivity and ductility in this UFG material and this is associated with grain boundary sliding and enhanced diffusion along the Al/Al grain boundaries which appear to be wetted by Zn-rich layers.
KW - Grain boundary sliding
KW - Micro and nanoindentation
KW - Strain rate sensitivity
KW - Ultrafine-grained materials
KW - Wetted boundaries
UR - http://www.scopus.com/inward/record.url?scp=84859214853&partnerID=8YFLogxK
U2 - 10.1016/j.msea.2012.02.056
DO - 10.1016/j.msea.2012.02.056
M3 - Article
AN - SCOPUS:84859214853
VL - 543
SP - 117
EP - 120
JO - Materials Science and Engineering: A
JF - Materials Science and Engineering: A
SN - 0921-5093
ER -
ID: 35168760