This study investigates the deposition of gallium oxide (Ga2O3) thin films by plasma-enhanced atomic layer deposition (PE-ALD) using nitrous oxide (N2O) as the oxidant for surface passivation of crystalline silicon. The deposition was performed at a low temperature of 75°C in a direct-plasma configuration, enabling conformal coating of substrates. Cross-sectional TEM confirmed the amorphous nature of the Ga2O3 films and the formation of a thin interfacial SiOx layer at the substrate interface. STEM-EDX elemental mapping showed a homogeneous distribution of gallium and oxygen, along with traces of nitrogen and carbon, attributed to precursor–plasma interactions. Optical measurements revealed an optical bandgap of 4.52 eV, consistent with literature values for amorphous Ga2O3. It was found that the growth per cycle increased from 0.41 to 0.84 Å/cycle with increasing plasma power; however, higher power and extended plasma exposure deteriorated the passivation quality due to plasma-induced damage at the Ga2O3/Si interface. The maximum effective minority carrier lifetime reached 443 μs at a plasma power of 10 W (22 mW/cm2), indicating highly efficient passivation under low-damage deposition conditions. These results demonstrate the potential of N2O-based PE-ALD Ga2O3 films as wide-bandgap, low-temperature passivation layers for next-generation silicon solar cells.
Original languageEnglish
Article number165092
JournalApplied Surface Science
Volume719
DOIs
StatePublished - 1 Feb 2026

    Research areas

  • Gallium oxide, N2O plasma, Optical bandgap, Plasma-enhanced atomic layer deposition, Silicon solar cells, Surface passivation

ID: 144820205