Control of TiN oxidation upon atomic layer deposition of oxides. / Filatova, E. O.; Sakhonenkov, S. S.; Konashuk, A. S.; Afanas'Ev, V. V.

In: Physical Chemistry Chemical Physics, Vol. 20, No. 44, 28.11.2018, p. 27975-27982.

Research output: Contribution to journalArticlepeer-review

Harvard

APA

Vancouver

Author

Filatova, E. O. ; Sakhonenkov, S. S. ; Konashuk, A. S. ; Afanas'Ev, V. V. / Control of TiN oxidation upon atomic layer deposition of oxides. In: Physical Chemistry Chemical Physics. 2018 ; Vol. 20, No. 44. pp. 27975-27982.

BibTeX

@article{294836cae49049019f2b13e244ba449b,
title = "Control of TiN oxidation upon atomic layer deposition of oxides",
abstract = "The interfaces of a physical-vapor deposited (PVD)-TiN electrode with atomic-layer deposited (ALD) HfO2 layers were studied using photoelectron spectroscopy with high kinetic energies of photoelectrons enabling nondestructive in-depth chemical profiling and phase analysis. Our results reveal the presence of only TiNxOy at the TiN/ALD-HfO2 interface with no measurable traces of the TiO2 phase. By contrast, the interface formed by ALD of HfO2 on top of PVD TiN contains both TiO2 and TiNxOy compounds and may be compared to an HfO2/TiN interface with intentional ALD TiO2 interlayer (IL) formation prior to HfO2 growth. Pre-growth of ALD Al2O3 IL drastically reduces the TiO2 and TiNxOy amounts present at the HfO2/TiN interface, which can be ascribed to oxygen scavenging from the initially oxidized TiN surface by energetically more favorable Al-O bonds. The present study demonstrates that the amount of TiO2 phase can be effectively controlled, i.e., increased or decreased, during the ALD process enabling engineering of vacancy-mediated processes.",
keywords = "SPECTRA, XPS",
author = "Filatova, {E. O.} and Sakhonenkov, {S. S.} and Konashuk, {A. S.} and Afanas'Ev, {V. V.}",
year = "2018",
month = nov,
day = "28",
doi = "10.1039/c8cp06076b",
language = "English",
volume = "20",
pages = "27975--27982",
journal = "Physical Chemistry Chemical Physics",
issn = "1463-9076",
publisher = "Royal Society of Chemistry",
number = "44",

}

RIS

TY - JOUR

T1 - Control of TiN oxidation upon atomic layer deposition of oxides

AU - Filatova, E. O.

AU - Sakhonenkov, S. S.

AU - Konashuk, A. S.

AU - Afanas'Ev, V. V.

PY - 2018/11/28

Y1 - 2018/11/28

N2 - The interfaces of a physical-vapor deposited (PVD)-TiN electrode with atomic-layer deposited (ALD) HfO2 layers were studied using photoelectron spectroscopy with high kinetic energies of photoelectrons enabling nondestructive in-depth chemical profiling and phase analysis. Our results reveal the presence of only TiNxOy at the TiN/ALD-HfO2 interface with no measurable traces of the TiO2 phase. By contrast, the interface formed by ALD of HfO2 on top of PVD TiN contains both TiO2 and TiNxOy compounds and may be compared to an HfO2/TiN interface with intentional ALD TiO2 interlayer (IL) formation prior to HfO2 growth. Pre-growth of ALD Al2O3 IL drastically reduces the TiO2 and TiNxOy amounts present at the HfO2/TiN interface, which can be ascribed to oxygen scavenging from the initially oxidized TiN surface by energetically more favorable Al-O bonds. The present study demonstrates that the amount of TiO2 phase can be effectively controlled, i.e., increased or decreased, during the ALD process enabling engineering of vacancy-mediated processes.

AB - The interfaces of a physical-vapor deposited (PVD)-TiN electrode with atomic-layer deposited (ALD) HfO2 layers were studied using photoelectron spectroscopy with high kinetic energies of photoelectrons enabling nondestructive in-depth chemical profiling and phase analysis. Our results reveal the presence of only TiNxOy at the TiN/ALD-HfO2 interface with no measurable traces of the TiO2 phase. By contrast, the interface formed by ALD of HfO2 on top of PVD TiN contains both TiO2 and TiNxOy compounds and may be compared to an HfO2/TiN interface with intentional ALD TiO2 interlayer (IL) formation prior to HfO2 growth. Pre-growth of ALD Al2O3 IL drastically reduces the TiO2 and TiNxOy amounts present at the HfO2/TiN interface, which can be ascribed to oxygen scavenging from the initially oxidized TiN surface by energetically more favorable Al-O bonds. The present study demonstrates that the amount of TiO2 phase can be effectively controlled, i.e., increased or decreased, during the ALD process enabling engineering of vacancy-mediated processes.

KW - SPECTRA

KW - XPS

UR - http://www.scopus.com/inward/record.url?scp=85056547333&partnerID=8YFLogxK

UR - http://xlink.rsc.org/?DOI=C8CP06076B

UR - http://www.mendeley.com/research/control-tin-oxidation-upon-atomic-layer-deposition-oxides

U2 - 10.1039/c8cp06076b

DO - 10.1039/c8cp06076b

M3 - Article

C2 - 30382269

AN - SCOPUS:85056547333

VL - 20

SP - 27975

EP - 27982

JO - Physical Chemistry Chemical Physics

JF - Physical Chemistry Chemical Physics

SN - 1463-9076

IS - 44

ER -

ID: 36187409