Atomic layer deposition for efficient oxygen evolution reaction at Pt/Ir catalyst layers

Stefanie Schlicht, Korcan Percin, Stefanie Kriescher, André Hofer, Claudia Weidlich, Matthias Wessling, Julien Bachmann

Результат исследований: Научные публикации в периодических изданияхстатьярецензирование

1 Цитирования (Scopus)

Аннотация

We provide a direct comparison of two distinct methods of Ti felt surface treatment and Pt/Ir electrocatalyst deposition for the positive electrode of regenerative fuel cells and vanadium-air redox flow batteries. Each method is well documented in the literature, and this paper provides a direct comparison under identical experimental conditions of electrochemical measurements and in identical units. In the first method, based on classical engineering, the bimetallic catalyst is deposited by dip-coating in a precursor solution of the salts followed by their thermal decomposition. In the alternative method, more academic in nature, atomic layer deposition (ALD) is applied to the felts after anodization. ALD allows for a controlled coating with ultralow noble-metal loadings in narrow pores. In acidic electrolyte, the ALD approach yields improved mass activity (557 A·g-1 as compared to 80 A·g-1 at 0.39 V overpotential) on the basis of the noble-metal loading, as well as improved stability.

Язык оригиналаанглийский
Страницы (с-по)952-959
Число страниц8
ЖурналBeilstein Journal of Nanotechnology
Том11
DOI
СостояниеОпубликовано - 2020

Предметные области Scopus

  • Материаловедение (все)
  • Физика и астрономия (все)
  • Электротехника и электроника

Fingerprint Подробные сведения о темах исследования «Atomic layer deposition for efficient oxygen evolution reaction at Pt/Ir catalyst layers». Вместе они формируют уникальный семантический отпечаток (fingerprint).

Цитировать