The processes of formation of the LaSr2Mn2O 7 compound are investigated in the temperature range 800-1400°C. The formation of the LaSr2Mn2O7 compound is found to occur through intermediate phases, namely, LaMnO3 and Sr2MnO4. It is revealed that the decomposition of the LaSr2Mn2O7 compound is caused by a decrease in both the temperature and the oxygen pressure.